dissolving nylon-6 and/or nylon-66
Author: Niraj Vasishtha
Date: Fri, 21 Aug 1992 15:14
Date: Fri, 21 Aug 1992 15:14
6 lines
644 bytes
644 bytes
I'm looking for a solvent or a combinations of two compatible solvent that would dissolve PET, nylon-6 and -66 without chemically degrading the material. would any one happen to have info in this regard? niraj vasishtha vasisn@rpi.edu
Re: dissolving nylon-6 and/or nylon-66
Author: William E. Johns;S23015
Date: Fri, 21 Aug 1992 16:18
Date: Fri, 21 Aug 1992 16:18
26 lines
1466 bytes
1466 bytes
In article <x-jytdh@rpi.edu> vasisn@rpi.edu writes:
>
> I'm looking for a solvent or a combinations of two compatible solvent that would dissolve PET, nylon-6 and -66 without chemically degrading the material.
> would any one happen to have info in this regard?
>
>niraj vasishtha
>vasisn@rpi.edu
>
Yep, try furfuryl alcohol. Heat it gently, without flame. I have dissolved
any number of different nylons in the stuff--a great solvent for this type
of polymer.
Enjoy,
Bill
________________________________________________________________
bill@wsuaix.csc.wsu.edu if you feel compelled to send email
johnsw@wsuvm1.csc.wsu.edu if you seriously expect an answer
AMA #500924 DoD #00314 WMTC #0002 SR= 2.125
FJ1200 R100GS/PD 740GLE KotV KotRR KotD #0001 :-)
\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/
If you understand, things are just as they are;
If you do not understand, things are just as they are.
Zen verse
Re: dissolving nylon-6 and/or nylon-66
Author: Steven Pollack
Date: Fri, 21 Aug 1992 21:49
Date: Fri, 21 Aug 1992 21:49
36 lines
1985 bytes
1985 bytes
In article <1992Aug21.161800.4727@serval.net.wsu.edu> bill@wsuaix.csc.wsu.edu (William E. Johns;S23015) writes: >In article <x-jytdh@rpi.edu> vasisn@rpi.edu writes: >> >> I'm looking for a solvent or a combinations of two compatible solvent that would dissolve PET, nylon-6 and -66 without chemically degrading the material. >> would any one happen to have info in this regard? >> >>niraj vasishtha >>vasisn@rpi.edu >> > >Yep, try furfuryl alcohol. Heat it gently, without flame. I have dissolved >any number of different nylons in the stuff--a great solvent for this type >of polymer. > >Enjoy, > >Bill >________________________________________________________________ >bill@wsuaix.csc.wsu.edu if you feel compelled to send email For all three, the best thing going is hexafluoroisopropanol. It dissolves the nylons and PET. It is expensive. But it works. We have done molecular weight analysis via GPC in this stuff, bu the solvent was donated. Cost about $4K / gallon!!! _______________________________________________________________________ Steven K. Pollack | University of Cincinnati | Department of Materials Science | I notice that you are still & Engineering | using polymers! 498 Rhodes Hall ML#12 | - Lt. Commander Montgomery Scott Cincinnati, OH 45221-0012 | U.S.S. Enterprise spollack@ester.mse.uc.edu | ________________________________________________________________________
Thread Navigation
This is a paginated view of messages in the thread with full content displayed inline.
Messages are displayed in chronological order, with the original post highlighted in green.
Use pagination controls to navigate through all messages in large threads.
Back to All Threads