Al honeycomb sandwitch panels
Author: STUART ROBERTS
Date: Thu, 08 Oct 1992 02:20
Date: Thu, 08 Oct 1992 02:20
6 lines
691 bytes
691 bytes
Can anyone suggest a suitable glue for the construction of Al honeycomb panels with Al skins. The operating environment is the same as that of a car. A glue that doesn't need temperatures above 200 C would be best. Thanks in advance, Stu.
Re: Al honeycomb sandwitch panels
Author: STEPANIAN, CHRISTOPHER JOHN
Date: Fri, 09 Oct 1992 15:55
Date: Fri, 09 Oct 1992 15:55
23 lines
1643 bytes
1643 bytes
In article <10616330.16.718510858@eng2.eng.monash.edu.au>, 10616330@eng2.eng.monash.edu.au (STUART ROBERTS) writes... >Can anyone suggest a suitable glue for the construction of Al honeycomb >panels with Al skins. The operating environment is the same as that of a >car. A glue that doesn't need temperatures above 200 C would be best. > >Thanks in advance, > Stu. A suitable solution to would be FM300, produced (I think) by American Cyanimid. Another product that is essentially the same thing is fabicated by 3M;I can't remember the product number. These products have brothers and sisters in the same line that have different material properties (shear modulus, cure temp, hydroscopic tendancies, etc...). You might be best off contacting these companies and requesting fact sheets on their whole 'sheet adhesive' line and then determine the best product for the conditions (including price) that the sandwich has to deal with. BTW the products are not cheap, but you can sometimes get samples that cover your needs. Good luck, Chris Stepanian Department of Ocean Engineering Texas A&M
Thread Navigation
This is a paginated view of messages in the thread with full content displayed inline.
Messages are displayed in chronological order, with the original post highlighted in green.
Use pagination controls to navigate through all messages in large threads.
Back to All Threads