I am planning to begin my senior thesis, and one possible topic that
interests me is the disposal of bauxite tailings (red mud) and fly ash
through some combination of the two, perhaps making bricks or agglomerates
for concrete.  I know a little about them, but I was wondering if anyone
had specific knowledge about this, or could provide some good references on
red mud, fly ash, or combinations.  Thank you.

						Tony Prats

prats@bigvax.alfred.edu		Tony.Prats@lambada.oit.unc.edu


--
   The opinions expressed are not necessarily those of the University of
     North Carolina at Chapel Hill, the Campus Office for Information
        Technology, or the Experimental Bulletin Board Service.
           internet:  laUNChpad.unc.edu or 152.2.22.80
Thread Navigation

This is a paginated view of messages in the thread with full content displayed inline.

Messages are displayed in chronological order, with the original post highlighted in green.

Use pagination controls to navigate through all messages in large threads.

Back to All Threads