Chemical thinning of GaAs
Author: gambit
Date: Tue, 12 Jan 1993 20:52
Date: Tue, 12 Jan 1993 20:52
19 lines
1422 bytes
1422 bytes
I am currently trying to improve TEM sample preparation for gallium arsenide specimens. My present method of production is by dimpling the GaAs to about 50 microns, and then using chemical thinning to produce an electron transparent region. However, I have not been getting very useful results after the chemical thinning. This is either a result of the thinning process itself (I am using sulfuric acid and hydrogen peroxide) or the cleaning process afterwards. The process is time-consuming as well. I would like to be able to improve it as much as possible, but am having difficulty finding any references on this technique. Does anyone know of any reference materials on chemical thinning of semiconductors? Please E-mail me if you do. Thanks in advance! ------------------------ Benjamin W. Lagow Grad Res Asst, Dept. of Materials Science and Engineering University of Illinois at Urbana-Champaign
Thread Navigation
This is a paginated view of messages in the thread with full content displayed inline.
Messages are displayed in chronological order, with the original post highlighted in green.
Use pagination controls to navigate through all messages in large threads.
Back to All Threads