I have just discovered that 3-n-butyl-pyridine forms a glass
somewhere between 125 K and 150 K. I have been unable to find any
reference giving a value for Tg or even admitting that it forms a glass
(I guessed that it would because butyl benzene does) after searching
through twenty years of Chem Abstracts plus a few other sources. Does
anyone out there have a reference giving Tg for this stuff? Barring
that, does anyone know where I could send a sample to have DSC done
on it? Thanks.
__________________________________________________________________________
John Fourkas jaco@ccwf.cc.utexas.edu
Department of Chemistry spike@d31mf0.stanford.edu
University of Texas at Austin jaco@leland.stanford.edu
Thread Navigation
This is a paginated view of messages in the thread with full content displayed inline.
Messages are displayed in chronological order, with the original post highlighted in green.
Use pagination controls to navigate through all messages in large threads.
Back to All Threads