Solvent for PVDF
Author: Timothy J. Drabik
Date: Thu, 30 Jul 1992 17:09
Date: Thu, 30 Jul 1992 17:09
9 lines
565 bytes
565 bytes
I'm looking for a solvent for polyvinylidene flouride. I would like to spin-deposit it. Can anyone recommend a journal reference or a chemical? Tim Drabik drabik@solaris.gatech.edu --
Re: Solvent for PVDF
Author: Barry Ornitz
Date: Fri, 31 Jul 1992 17:53
Date: Fri, 31 Jul 1992 17:53
30 lines
2161 bytes
2161 bytes
In article <1992Jul30.170903.12107@ee.gatech.edu> drabik@eecom.gatech.edu (Timothy J. Drabik) writes: >I'm looking for a solvent for polyvinylidene flouride. >I would like to spin-deposit it. Can anyone recommend >a journal reference or a chemical? PVDF is used extensively in the chemical industry because of its chemical resistance to most materials. In fact, it is used as a replacement for PTFE (Teflon) in many applications because of superior mechanical properties with only a slight decrease in chemical resistance. Finding a solvent for polyvinylidene difluoride will be very difficult. Having said this, however, I will add that one of our commercial high boiling point solvents, Ektasolve EEP, has been known to attack PVDF. In our manufacturing process for EEP, Kynar (PVDF) coated pH probes were dissolved away completely as were Kynar insulated electrical conductivity probes. I am not sure this solvent will meet your needs however. Why do most net posters always mistakenly spell fluorine containing compounds as if they were bakery products? ;-) Barry ----------------- | ___ ________ | Dr. Barry L. Ornitz WA4VZQ | | / / | | Eastman Kodak Company | | / / | | Eastman Chemical Company Research Laboratories | |< < K O D A K| | Process Instrumentation Research Laboratory | | \ \ | | P. O. Box 1972, Building 167B | |__\ \________| | Kingsport, TN 37662 615/229-4904 | | INTERNET: ornitz@kodak.com -----------------
Re: Solvent for PVDF
Author: Tom Knight
Date: Fri, 31 Jul 1992 21:35
Date: Fri, 31 Jul 1992 21:35
8 lines
866 bytes
866 bytes
(Timothy J. Drabik) writes: I'm looking for a solvent for polyvinylidene flouride. I would like to spin-deposit it. Can anyone recommend a journal reference or a chemical? Perhaps it would be possible to spin the monomer and polymerize it in situ. The down side is that the monomer is probably incredibly toxic.
Re: Solvent for PVDF
Author: Kip D. Hauch
Date: Thu, 06 Aug 1992 23:29
Date: Thu, 06 Aug 1992 23:29
25 lines
1173 bytes
1173 bytes
Caldwell spin casts polymer blends of PMMA and PVDF from 2%w/v solutions in DMAc onto glass disks (coverslips) although I am unsure whether pure PVDF was used much in this work. Surface Characterization of Polymer Blends: Acid/Base Considerations in Static SIMS Sean J. Caldwell M.S. Thesis 1990. Dept. of Chemical Engineering University of Washington In article <1992Jul30.170903.12107@ee.gatech.edu>, drabik@eecom.gatech.edu (Timothy J. Drabik) writes: > > I'm looking for a solvent for polyvinylidene flouride. > I would like to spin-deposit it. Can anyone recommend > a journal reference or a chemical? > > Tim Drabik > drabik@solaris.gatech.edu > > > -- > >
Re: Solvent for PVDF
Author: CHEBURZY
Date: Tue, 11 Aug 1992 03:56
Date: Tue, 11 Aug 1992 03:56
54 lines
3118 bytes
3118 bytes
In article <1992Jul31.175332.10341@kodak.kodak.com> ornitz@kodak.kodak.com (Barry Ornitz) writes: > >In article <1992Jul30.170903.12107@ee.gatech.edu> drabik@eecom.gatech.edu >(Timothy J. Drabik) writes: >>I'm looking for a solvent for polyvinylidene flouride. >>I would like to spin-deposit it. Can anyone recommend >>a journal reference or a chemical? > >PVDF is used extensively in the chemical industry because of its chemical >resistance to most materials. In fact, it is used as a replacement for PTFE >(Teflon) in many applications because of superior mechanical properties with >only a slight decrease in chemical resistance. Finding a solvent for >polyvinylidene difluoride will be very difficult. > >Having said this, however, I will add that one of our commercial high boiling >point solvents, Ektasolve EEP, has been known to attack PVDF. In our >manufacturing process for EEP, Kynar (PVDF) coated pH probes were dissolved >away completely as were Kynar insulated electrical conductivity probes. I >am not sure this solvent will meet your needs however. > >Why do most net posters always mistakenly spell fluorine containing compounds >as if they were bakery products? ;-) > Barry > ----------------- >| ___ ________ | Dr. Barry L. Ornitz WA4VZQ >| | / / | | Eastman Kodak Company >| | / / | | Eastman Chemical Company Research Laboratories >| |< < K O D A K| | Process Instrumentation Research Laboratory >| | \ \ | | P. O. Box 1972, Building 167B >| |__\ \________| | Kingsport, TN 37662 615/229-4904 >| | INTERNET: ornitz@kodak.com > ----------------- Polyvinylidene difluoride (PVDF) has been extensively researched in early 1980's because of on of its crystallographic form which is piezoelectric. This form, made by Penwalt (sp?) Corp. under tradename KYNAR, has found many applications as thin film piezoelectric transducer. I don't know how Penwalt makes it but I remember casting PVDF films for my Raman studies. The solvents I used were hexane and acetone. As Dr. Ornitz mentioned it is not readily soluble and some patience is needed. However, for spincoating technique the above solvents aren't the ideal one. I would suggest to start with low molecular weight polymer (Aldrich) in form of powder rather than pellets. Filtering the solution is another problem and may cause some gray hair grow. For more info I would scan Chem Abs (1980-4). Unfortunately I don't have references I used for my work anymore. Regards, Ryszard Burzynski
Thread Navigation
This is a paginated view of messages in the thread with full content displayed inline.
Messages are displayed in chronological order, with the original post highlighted in green.
Use pagination controls to navigate through all messages in large threads.
Back to All Threads