Re: Insulator with good heat conductivity

#194
From: Scott Hannahs
Date: Wed, 12 Aug 1992 23:01
14 lines
1239 bytes
<Lots of arguments about BeO deleted>

As a low temp kind o' guy, why not use copper with a covering of
cigarette papers.  Every cryogenic tool kit has a set of rolling papers.
You can hold them in place with the standard GE varnish (7031).  This
has a breakdown voltage of several (~200-300) V/mil (that's 0.001 inch).

The easiest way to get thermal conductivity is to make the insulator
much thinner.  The problem you might have at high voltage is the ease
with which He gas breaks down.  There is a minimum in the breakdown
voltage around 10 torr and so make sure your leads are well insulated
above the liquid near the top of the cryostat.

Scott Hannahs, F. Bitter National Magnet Lab, sth@slipknot.mit.edu
Technical Details
Message-ID: <sth.713660510@slipknot.mit.edu>
Path: arc1-ca.pugleaf.net!sparky!uunet!snorkelwacker.mit.edu!bloom-picayune.mit.edu!slipknot.mit.edu!sth
References: <7926@dirac.physics.purdue.edu> <17760005@hpnmdla.sr.hp.com>

Show Full Headers
Complete Article Headers
Newsgroups: sci.materials
Path: arc1-ca.pugleaf.net!sparky!uunet!snorkelwacker.mit.edu!bloom-picayune.mit.edu!slipknot.mit.edu!sth
From: sth@slipknot.mit.edu (Scott Hannahs)
Subject: Re: Insulator with good heat conductivity
Message-ID: <sth.713660510@slipknot.mit.edu>
Sender: news@athena.mit.edu (News system)
Nntp-Posting-Host: slipknot.mit.edu
Organization: Massachvsetts Institvte of Technology
References: <7926@dirac.physics.purdue.edu> <17760005@hpnmdla.sr.hp.com>
Date: Wed, 12 Aug 1992 23:01:50 GMT
Lines: 15