Since there was some response to a recent request for the properties
of silicon nitride, I thought I'd post a similar request.  Does anyone
have any information on the properties of titanium nitride?  I'm
particularly interested in the strength of the material (yield
strength, rupture strength, etc.).  Any numbers and or references
would be helpful.

   Thanks,
--

   jake blanchard -- university of wisconsin - madison
   blanchard@engr.wisc.edu  OR   jake@nucst6.neep.wisc.edu
Re: Properties of titanium nitride
#264
Author: Dong Liu
Date: Thu, 12 Nov 1992 04:45
25 lines
1521 bytes
In article <JAKE.92Nov11155601@nucst6.neep.wisc.edu> jake@nucst6.neep.wisc.edu (james blanchard) writes:
>
>Since there was some response to a recent request for the properties
>of silicon nitride, I thought I'd post a similar request.  Does anyone
>have any information on the properties of titanium nitride?  I'm
>particularly interested in the strength of the material (yield
>strength, rupture strength, etc.).  Any numbers and or references
>would be helpful.
>
>   Thanks,
>--
>
>   jake blanchard -- university of wisconsin - madison
>   blanchard@engr.wisc.edu  OR   jake@nucst6.neep.wisc.edu
>

I have some good references as follows:
"Material selection for  hard coatings"
J.Voc.Sci.Tec.A 4 (6), pp.2661-2669,(1986)
  
"The deposition and film properties of reactively sputtered Titanium
Nitride" ,  R.C. Ellwanger and J.M. Towner,
Thin Solid Films 161, (1988), pp.289-304.
   
Good luck to you.
Re: Properties of titanium nitride
#268
Author: Mansig Kim
Date: Fri, 13 Nov 1992 15:55
26 lines
1354 bytes
In article <JAKE.92Nov11155601@nucst6.neep.wisc.edu> jake@nucst6.neep.wisc.edu (james blanchard) writes:
>
>Since there was some response to a recent request for the properties
>of silicon nitride, I thought I'd post a similar request.  Does anyone
>have any information on the properties of titanium nitride?  I'm
>particularly interested in the strength of the material (yield
>strength, rupture strength, etc.).  Any numbers and or references
>would be helpful.
>
>   Thanks,
>--
>
>   jake blanchard -- university of wisconsin - madison
>   blanchard@engr.wisc.edu  OR   jake@nucst6.neep.wisc.edu


Since we have many requests about materials properties, do we have 
ftp site or free access site that provides properties information?

I also need many materials properties. If I post news to get property
information everytime I need, it will consume lots of news resources.


Regards,

Mansig
Thread Navigation

This is a paginated view of messages in the thread with full content displayed inline.

Messages are displayed in chronological order, with the original post highlighted in green.

Use pagination controls to navigate through all messages in large threads.

Back to All Threads