2 plastics questions
#182
Author: John E. Brennan
Date: Mon, 31 Aug 1992 16:59
21 lines
948 bytes
I'm hoping somebody can give me some help with these questions.

1.  What adhesives can bond high density polyethylene to rigid PVC or 
    HDPE to itself?  The bonds would be used in outdoor applications.

2.  What plastics would be resistant to soaking in hot transmission fluid?


Any help or guidance would be greatly appreciated.  Thanks a lot!

Take Care,
 
John 



----------------------------------------------------------------------------
                            
John Brennan 

a750288@pan.mc.ti.com 
Re: 2 plastics questions
#184
Author: William E. Johns;S23015
Date: Mon, 31 Aug 1992 20:49
27 lines
1671 bytes
In article <a750288.16@pan.mc.ti.com> a750288@pan.mc.ti.com (John E. Brennan) writes:
>I'm hoping somebody can give me some help with these questions.
>
>1.  What adhesives can bond high density polyethylene to rigid PVC or 
>    HDPE to itself?  The bonds would be used in outdoor applications.

I would guess that your best luck would be in bonding HDPE to PVC or itself
would be with HDPE itself.  Use it as a hot melt.

>2.  What plastics would be resistant to soaking in hot transmission fluid?

I just gotto believe there are lots and lots.  How hot?  Nylons, delrin,
PTFE, what's the application?
>
Ride Free,

Bill
________________________________________________________________
bill@wsuaix.csc.wsu.edu if you feel compelled to send email
johnsw@wsuvm1.csc.wsu.edu if you seriously expect an answer
AMA #500924   DoD #00314   WMTC #0002   SR= 2.125
FJ1200 R100GS/PD 740GLE  KotV KotRR KotD #0001  :-)
\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/

An adventure is only an inconvenience rightly understood.
An inconvenience is only an adventure wrongly considered.
                                               Chesterton
Re: 2 plastics questions
#193
Author: John E. Brennan
Date: Fri, 04 Sep 1992 13:14
34 lines
1621 bytes
In article <1992Aug31.204952.29444@serval.net.wsu.edu> bill@wsuaix.csc.wsu.edu (William E. Johns;S23015) writes:
>In article <a750288.16@pan.mc.ti.com> a750288@pan.mc.ti.com (John E. Brennan) writes:
>>I'm hoping somebody can give me some help with these questions.
>>
>>1.  What adhesives can bond high density polyethylene to rigid PVC or 
>>    HDPE to itself?  The bonds would be used in outdoor applications.

>I would guess that your best luck would be in bonding HDPE to PVC or itself
>would be with HDPE itself.  Use it as a hot melt.


THANKS A BUNCH FOR THIS!!  We've made up a few samples using a hot melt and
they're doing great.

>>2.  What plastics would be resistant to soaking in hot transmission fluid?

>I just gotto believe there are lots and lots.  How hot?  Nylons, delrin,
>PTFE, what's the application?
>>

The application is a casing for an electrical part inside a transmission.
Temperature would be 250 F or above.

Take Care,
 
John 



----------------------------------------------------------------------------
                            
John Brennan 

a750288@pan.mc.ti.com 
Re: 2 plastics questions
#160
Author: William E. Johns;S23015
Date: Mon, 07 Sep 1992 16:15
51 lines
2760 bytes
In article <a750288.19@pan.mc.ti.com> a750288@pan.mc.ti.com (John E. Brennan) writes:
>In article <1992Aug31.204952.29444@serval.net.wsu.edu> bill@wsuaix.csc.wsu.edu (William E. Johns;S23015) writes:
>>In article <a750288.16@pan.mc.ti.com> a750288@pan.mc.ti.com (John E. Brennan) writes:
>>>I'm hoping somebody can give me some help with these questions.
>>>
>>>1.  What adhesives can bond high density polyethylene to rigid PVC or 
>>>    HDPE to itself?  The bonds would be used in outdoor applications.
>
>>I would guess that your best luck would be in bonding HDPE to PVC or itself
>>would be with HDPE itself.  Use it as a hot melt.
>
>
>THANKS A BUNCH FOR THIS!!  We've made up a few samples using a hot melt and
>they're doing great.

Good.
>
>>>2.  What plastics would be resistant to soaking in hot transmission fluid?
>
>>I just gotto believe there are lots and lots.  How hot?  Nylons, delrin,
>>PTFE, what's the application?
>>>
>
>The application is a casing for an electrical part inside a transmission.
>Temperature would be 250 F or above.

Hmmmm.  This could be interesting.  I suspect that any number of polymers are
stable to that environment, but if you are gonna try and seal something
inside of a container, then your seal will be suspect.  Tranny oil just
isn't all that expenseive.  Get yourself some chunks of various polymers, 
machine them out to a smallish edge and treat with hot tranny fluid for a bit.
By knowing the dimensions and weights before you start, you can determine
which materials has the least uptake and is the most dimensionally stable.
Take the toughest one and make your container using a really good o-ring.

Ride Free,

Bill
________________________________________________________________
bill@wsuaix.csc.wsu.edu if you feel compelled to send email
johnsw@wsuvm1.csc.wsu.edu if you seriously expect an answer
AMA #500924   DoD #00314   WMTC #0002   SR= 2.125
Yamabeemer fjgs1200pdr100 740GLE  KotV KotRR KotD #0001  :-)
\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/\/

If you walk, just walk.
If you sit, just sit.
If you ride, just ride.

Above all, don't wobble.
                             Zen saying (slightly modified)
Thread Navigation

This is a paginated view of messages in the thread with full content displayed inline.

Messages are displayed in chronological order, with the original post highlighted in green.

Use pagination controls to navigate through all messages in large threads.

Back to All Threads